Properti | Satuan | CBZSD-30. | CBZSD-35. | CBZSD-40. | CBZSD-50. | Tesmetode |
Ketebalan | mm. | 0,30 ± 0,03. | 0,35 ± 0,03. | 0,40 ± 0,03. | 0.50 ± 0,03. | ISO 9073-2. |
Massaper unit area. | g / m2. | 110 ± 10. | 120 ± 10. | 130 ± 10. | 160 ± 10. | ISO 9073-2. |
Tarikkekuatan | N / cm. | ³30. | ³35. | ³40. | ³50. | ISO 9073-3. |
Pemanjangan | % | ³12. | ³12. | ³12. | ³12. | ISO 9073-3. |
Kecepatan pembengkakan | mm / 1'0 '' | ³8. | ³9. | ³10. | ³12. | GB 450. |
Tinggi pembengkakan. | mm / 3'00 ' | ³12. | ³13. | ³14. | ³16. | GB 450. |
Stabilitas jangka pendek | ° C. | 230 | 230 | 230 | 230 | Q / Tr.J02.01-2000. |
Stabilitas jangka panjang | ° C. | 90 | 90 | 90 | 90 | IEC 216-1990. |
Resistensi permukaan. | W | £ 1500. | £ 1500. | £ 1500. | £ 1500. | GB 3048. |
VolumePerlawanan | W.cm. | <1x106. | <1x106. | <1x106. | <1x106. | GB 3048. |
Kelembaban.isi | % | £ 9. | £ 9. | £ 9. | £ 9. | ISO 287. |
Properti | Satuan | CBZSD-25. | CBZSD-35.N | CBZSD-40.N | CBZSD-50.N | Metode pengujian |
Ketebalan | mm. | 0,25 ± 0,03. | 0,35 ± 0,03. | 0,40 ± 0,03. | 0.50 ± 0,03. | ISO 9073-2. |
Massaper unit area. | g / m2. | 100 ± 10. | 130 ± 10. | 140 ± 10. | 170 ± 10. | ISO 9073-2. |
Tarikkekuatan | N / cm. | ³25. | ³35. | ³40. | ³50. | ISO 9073-3. |
Pemanjangan | % | ³12. | ³12. | ³12. | ³12. | ISO 9073-3. |
Kecepatan pembengkakan | mm / 1'0 '' | ³7. | ³12. | ³12. | ³13. | GB 450. |
Tinggi pembengkakan. | mm / 3'00 ' | ³10. | ³15. | ³16. | ³18. | GB 450. |
Stabilitas jangka pendek | ° C. | 230 | 230 | 230 | 230 | Q / Tr.J02.01-2000. |
Stabilitas jangka panjang | ° C. | 90 | 90 | 90 | 90 | IEC 216-1990. |
Resistensi permukaan. | W | £ 1500. | £ 1500. | £ 1500. | £ 1500. | GB 3048. |
VolumePerlawanan | W.cm. | <1x106. | <1x106. | <1x106. | <1x106. | GB 3048. |
Kelembaban.isi | % | £ 9. | £ 9. | £ 9. | £ 9. | ISO 287. |
Properti | Satuan | CBZSD-30. | CBZSD-35. | CBZSD-40. | CBZSD-50. | Tesmetode |
Ketebalan | mm. | 0,30 ± 0,03. | 0,35 ± 0,03. | 0,40 ± 0,03. | 0.50 ± 0,03. | ISO 9073-2. |
Massaper unit area. | g / m2. | 110 ± 10. | 120 ± 10. | 130 ± 10. | 160 ± 10. | ISO 9073-2. |
Tarikkekuatan | N / cm. | ³30. | ³35. | ³40. | ³50. | ISO 9073-3. |
Pemanjangan | % | ³12. | ³12. | ³12. | ³12. | ISO 9073-3. |
Kecepatan pembengkakan | mm / 1'0 '' | ³8. | ³9. | ³10. | ³12. | GB 450. |
Tinggi pembengkakan. | mm / 3'00 ' | ³12. | ³13. | ³14. | ³16. | GB 450. |
Stabilitas jangka pendek | ° C. | 230 | 230 | 230 | 230 | Q / Tr.J02.01-2000. |
Stabilitas jangka panjang | ° C. | 90 | 90 | 90 | 90 | IEC 216-1990. |
Resistensi permukaan. | W | £ 1500. | £ 1500. | £ 1500. | £ 1500. | GB 3048. |
VolumePerlawanan | W.cm. | <1x106. | <1x106. | <1x106. | <1x106. | GB 3048. |
Kelembaban.isi | % | £ 9. | £ 9. | £ 9. | £ 9. | ISO 287. |
Properti | Satuan | CBZSD-25. | CBZSD-35.N | CBZSD-40.N | CBZSD-50.N | Metode pengujian |
Ketebalan | mm. | 0,25 ± 0,03. | 0,35 ± 0,03. | 0,40 ± 0,03. | 0.50 ± 0,03. | ISO 9073-2. |
Massaper unit area. | g / m2. | 100 ± 10. | 130 ± 10. | 140 ± 10. | 170 ± 10. | ISO 9073-2. |
Tarikkekuatan | N / cm. | ³25. | ³35. | ³40. | ³50. | ISO 9073-3. |
Pemanjangan | % | ³12. | ³12. | ³12. | ³12. | ISO 9073-3. |
Kecepatan pembengkakan | mm / 1'0 '' | ³7. | ³12. | ³12. | ³13. | GB 450. |
Tinggi pembengkakan. | mm / 3'00 ' | ³10. | ³15. | ³16. | ³18. | GB 450. |
Stabilitas jangka pendek | ° C. | 230 | 230 | 230 | 230 | Q / Tr.J02.01-2000. |
Stabilitas jangka panjang | ° C. | 90 | 90 | 90 | 90 | IEC 216-1990. |
Resistensi permukaan. | W | £ 1500. | £ 1500. | £ 1500. | £ 1500. | GB 3048. |
VolumePerlawanan | W.cm. | <1x106. | <1x106. | <1x106. | <1x106. | GB 3048. |
Kelembaban.isi | % | £ 9. | £ 9. | £ 9. | £ 9. | ISO 287. |
Tambahkan: 20 / Fl., 26 Jalan Zhongshan Utara, Nanjing, Jiangsu, Cina
Tel: 0086-25-83317070
Faks: 0086-25-83303377
Surel:peter@jocmachinery.com
Hak Cipta 2021 JOC Machinery Co., Ltd. Semua hak dilindungi undang-undang. Peta Situs Teknologi Oleh Leadong
Dilarang memperbanyak tanpa izin.